ASTM A240
Glomet Stainless stocks cold rolled and hot rolled sheets in austenitic stainless steel, duplex, titanium and nickel alloys at our Kalamboli yard. Sheets are supplied to ASTM A240 / ASME SA240 for stainless and duplex grades, ASTM B265 for titanium and the relevant ASTM B specification for each nickel alloy.
Standard 4×8 ft and 1250×2500 mm sheets are held in common grades, and we shear, laser or plasma cut to your drawing so you pay for the size you use. Every lot ships with the mill test certificate for its heat number.
The workhorse range — 304 for general fabrication, 316L where chlorides are present, 321 and 310S for heat.
304/304L316/316L321310S904LRoughly twice the yield strength of 316L with better resistance to pitting and stress corrosion cracking.
S31803S32205S32750S32760Commercially pure grades for seawater and chemical duty; Gr 5 (Ti-6Al-4V) where strength-to-weight matters.
Gr 1Gr 2Gr 5Gr 7Gr 12For high temperature, reducing acids and severe chloride service where stainless steel is not enough.
Inconel 600/625Incoloy 800/825Monel 400C276Ni 200| Grade | C | Mn | Si | P | S | Cr | Ni | Mo | N | Other |
|---|---|---|---|---|---|---|---|---|---|---|
| 304 | 0.08 | 2.00 | 0.75 | 0.045 | 0.030 | 18.0–20.0 | 8.0–10.5 | – | 0.10 | – |
| 304L | 0.030 | 2.00 | 0.75 | 0.045 | 0.030 | 17.5–19.5 | 8.0–12.0 | – | 0.10 | – |
| 316 | 0.08 | 2.00 | 0.75 | 0.045 | 0.030 | 16.0–18.0 | 10.0–14.0 | 2.00–3.00 | 0.10 | – |
| 316L | 0.030 | 2.00 | 0.75 | 0.045 | 0.030 | 16.0–18.0 | 10.0–14.0 | 2.00–3.00 | 0.10 | – |
| 321 | 0.08 | 2.00 | 0.75 | 0.045 | 0.030 | 17.0–19.0 | 9.0–12.0 | – | 0.10 | Ti 5×(C+N) – 0.70 |
| 310S | 0.08 | 2.00 | 1.50 | 0.045 | 0.030 | 24.0–26.0 | 19.0–22.0 | – | – | – |
| 904L | 0.020 | 2.00 | 1.00 | 0.045 | 0.035 | 19.0–23.0 | 23.0–28.0 | 4.0–5.0 | 0.10 | Cu 1.0–2.0 |
| Duplex 2205 (S32205) | 0.030 | 2.00 | 1.00 | 0.030 | 0.020 | 22.0–23.0 | 4.5–6.5 | 3.0–3.5 | 0.14–0.20 | – |
| Super Duplex 2507 (S32750) | 0.030 | 1.20 | 0.80 | 0.035 | 0.020 | 24.0–26.0 | 6.0–8.0 | 3.0–5.0 | 0.24–0.32 | Cu 0.50 |
| Grade | Ni | Cr | Mo | Fe | Cu | C | Mn | Si | Other |
|---|---|---|---|---|---|---|---|---|---|
| Titanium Gr 2 | – | – | – | 0.30 | – | 0.08 | – | – | O 0.25, N 0.03, H 0.015, Ti bal. |
| Titanium Gr 5 | – | – | – | 0.40 | – | 0.08 | – | – | Al 5.5–6.75, V 3.5–4.5, O 0.20, Ti bal. |
| Inconel 600 | 72.0 min | 14.0–17.0 | – | 6.0–10.0 | 0.50 | 0.15 | 1.00 | 0.50 | S 0.015 |
| Inconel 625 | 58.0 min | 20.0–23.0 | 8.0–10.0 | 5.0 | – | 0.10 | 0.50 | 0.50 | Nb+Ta 3.15–4.15 |
| Incoloy 800 | 30.0–35.0 | 19.0–23.0 | – | 39.5 min | 0.75 | 0.10 | 1.50 | 1.00 | Al 0.15–0.60, Ti 0.15–0.60 |
| Incoloy 825 | 38.0–46.0 | 19.5–23.5 | 2.5–3.5 | 22.0 min | 1.5–3.0 | 0.05 | 1.00 | 0.50 | Ti 0.6–1.2 |
| Monel 400 | 63.0 min | – | – | 2.50 | 28.0–34.0 | 0.30 | 2.00 | 0.50 | S 0.024 |
| Hastelloy C276 | Balance | 14.5–16.5 | 15.0–17.0 | 4.0–7.0 | – | 0.010 | 1.00 | 0.08 | W 3.0–4.5, Co 2.5 |
| Nickel 200 | 99.0 min | – | – | 0.40 | 0.25 | 0.15 | 0.35 | 0.35 | S 0.01 |
Weight %, maximum unless a range is shown. The mill test certificate supplied with each heat is the controlling document.
| Grade | Tensile Strength (MPa, min) | Yield Strength 0.2% (MPa, min) | Elongation (% in 50 mm, min) | Hardness (max) |
|---|---|---|---|---|
| 304 | 515 | 205 | 40 | 201 HBW / 92 HRB |
| 304L | 485 | 170 | 40 | 201 HBW / 92 HRB |
| 316 | 515 | 205 | 40 | 217 HBW / 95 HRB |
| 316L | 485 | 170 | 40 | 217 HBW / 95 HRB |
| 321 | 515 | 205 | 40 | 217 HBW / 95 HRB |
| 310S | 515 | 205 | 40 | 217 HBW / 95 HRB |
| 904L | 490 | 220 | 35 | 90 HRB |
| Duplex 2205 (S32205) | 655 | 450 | 25 | 293 HBW / 31 HRC |
| Super Duplex 2507 (S32750) | 795 | 550 | 15 | 310 HBW / 32 HRC |
| Grade | Tensile Strength (MPa, min) | Yield Strength 0.2% (MPa, min) | Elongation (%, min) | Condition |
|---|---|---|---|---|
| Titanium Gr 2 | 345 | 275 | 20 | Annealed |
| Titanium Gr 5 | 895 | 828 | 10 | Annealed |
| Inconel 600 | 550 | 240 | 30 | Annealed |
| Inconel 625 | 827 | 414 | 30 | Annealed (Grade 1) |
| Incoloy 800 | 520 | 205 | 30 | Annealed |
| Incoloy 825 | 586 | 241 | 30 | Annealed |
| Monel 400 | 483 | 193 | 35 | Annealed |
| Hastelloy C276 | 690 | 283 | 40 | Solution Annealed |
| Nickel 200 | 380 | 103 | 40 | Annealed |
Room temperature values for annealed sheet. Limits can vary with thickness — confirm against the ordered specification.





Tell us the grade, thickness, sheet size, finish and quantity. We quote with stock availability and delivery time.